Polymolecularity of the extremely high molecular mass polymer prepared by emulsion polymerization with a macromolecular initiator forming a heterogeneous phase

L. Šoltés, D. Mikulášová, J. Susla, and I. Hudec

Institute of Experimental Pharmacology, Slovak Academy of Sciences, 881 05 Bratislava

 

Abstract: Extremely high mol. wt. polystyrene  samples [Mw = (8.84-29.4) × 106] were prepd. by emulsion polymn. with a macromol. initiator forming a heterogeneous phase. The dependences of the monomer conversion, Mw, and Mw/Mn on the concns. of the initiator (x1), of the activator (x2), and of the emulsifier (x3) as well as on the polymn. temp. (x4) were tested by a factor expt. of the half-replica type 2(4-1). The true functional dependences of the studied output parameters on x1, x2, and x3 were math. approximated by a rotatable factor expt. At conditions under which the samples attained a local min. of polymolecularity (Mw/Mw,calc = 1.552) a poly(Me methacrylate)   sample was also synthesized.

Full paper in Portable Document Format: 354a533.pdf

 

Chemical Papers 35 (4) 533–541 (1981)

Wednesday, October 16, 2019

IMPACT FACTOR 2018
1.246
SCImago Journal Rank 2018
0.274
SEARCH
Advanced
VOLUMES
International Conference on Coordination and Bioinorganic Chemistry
46th International Conference of SSCHE
© 2019 Chemical Papers