Investigation of surface modified collagen biopolymer and natural leaf fibre reinforced biocomposite and their effects on tensile, flexural, impact, hardness, fatigue, creep, water absorption and drilling

Piyush Singhal, Vinod Kumar Naidu Pamuluri, Vibhor Mahajan, Romil Jain, M. Sreenivasa Reddy, Shree Jayaram K, V. Mohanavel, Sathish Kannan, and Seeniappan Kaliappan

Department of Mechanical Engineering, Institute of Engineering and Technology, GLA University, Mathura, India

 

E-mail: piyush_singhal2026@outlook.com

Received: 11 March 2026  Accepted: 14 June 2026

Abstract:

This study develops sustainable vinyl ester composites by valorising squid skin-derived cellular collagen waste and reinforcing it with abaca fibres, with a focus on improving interfacial bonding through silane surface treatment and enhancing resistance to environmental aging (seawater, tap water, and elevated temperatures), particularly under high-speed drilling conditions. The composites were fabricated using the hand layup method incorporating vinyl ester resin, abaca fibres, and squid skin cellular collagen particles. Silane-treated systems exhibited improved fibre-matrix adhesion, resulting in enhanced mechanical performance, fatigue response, creep resistance, and drilling stability under both unaged and aged conditions. The composite containing 57 vol% vinyl ester resin, 40 vol% abaca fiber and 3 vol% silane-treated collagen (V13) showed the best overall performance, achieving tensile strength of 135 MPa, flexural strength of 180 MPa, impact strength of 4.80 J, hardness of 82 shore-D, fatigue life of 24,711 cycles (25% UTS) and improved drilling quality with lower hole diameters of 3.06 mm (3 mm drill) and 6.08 mm (6 mm drill). Even under aging, V53 (60 °C, 3 vol% SCC) maintained superior durability, showing 108 MPa tensile strength, 144 MPa flexural strength, 3.84 J impact strength, 19,769 fatigue cycles, and controlled drilling damage with hole diameters of 3.52 and 6.99 mm, indicating excellent property retention. It also demonstrated improved fatigue resistance relative to reported natural fibre-reinforced vinyl ester composites, along with reduced creep deformation under sustained loading. Drilling tests indicated lower kerf formation, reflecting improved machining precision, while water absorption remained minimal, confirming improved moisture resistance. After aging exposure, silane-treated composites retained significantly better mechanical and functional properties than untreated counterparts, indicating effective mitigation of hydrothermal and thermal degradation. Microstructural analysis confirmed reduced voids, uniform filler dispersion, and improved interfacial bonding, while drilling damage analysis showed reduced delamination and fibre pull-out. Overall, the study demonstrates that silane modification combined with bio-waste-derived reinforcements provides a viable route for developing durable and sustainable composites for structural and machining-intensive applications. These composites are suitable for marine, automotive, aerospace, and construction applications due to their high mechanical strength, fatigue resistance, and durability under moisture and thermal aging.Their improved drilling performance and reduced delamination also make them ideal for precision-machined structural components requiring reliable fastening and long-term service stability.

Keywords: Composite; Polymer; Surface; Fibre; Fatigue properties; Creepbehaviour

Full paper is available at www.springerlink.com.

DOI: 10.1007/s11696-026-05217-2

 

Chemical Papers 80 (12) 14405–14420 (2026)

Tuesday, November 24, 2026